Phase Angle and Percent Heat

50% heat
dashed = full AC sine wave  ·  orange = what the SCRs let through

Firing delay
90°
Conducting
50% of each ½ cycle
Weld time
5 cyc · 0.083 s

Try:

How percent heat works. A single-phase resistance welding control uses a pair of SCRs as a fast electrical switch. Every half-cycle of the AC line, the SCRs wait, then fire. Once fired, they conduct until the current returns to zero at the end of that half-cycle.

Lower heat = later firing. At 100% heat the SCRs fire right at the start of each half-cycle and pass the full sine wave. At 50% they wait a quarter cycle (90°) and pass only the back half. At low heat they fire late and pass only a thin sliver.

Heat vs. weld time. Heat controls how much of each cycle gets through. Weld time (in cycles, 60 per second) controls how many cycles you get. Both together set the energy delivered to the weld.

Simplified drawing for illustration. On a real welder the transformer’s inductance shifts the current waveform, and the current does not scale one-for-one with percent heat. Questions? Call Spot Weld at (800) 582-5229.

What the current actually does

Inductance changes the picture. The chart above shows the voltage the SCRs let through. But a welding transformer is mostly inductance. Current lags behind voltage. Once the SCRs fire, current keeps flowing past the end of the half-cycle. It stops only when the current itself returns to zero.

0°180°360°

Line voltageVoltage the transformer seesWeld currentPower factor angle (full heat)Current returns to zero
Firing delay
–
When the control fires. Goes down with heat.
Conduction angle
–
How long current flows. Many weld meters call this “firing angle.”
Weld current
–
RMS, % of the most this machine can deliver.

Weld current vs. percent heat

No added current100%50%0%0%25%50%75%100%Percent heat

Weld currentOne-for-one (what the simple drawing suggests)

← Less inductive: short, small throat, little or no steel insideMore inductive: deep, wide throat, lots of steel inside →
Try:

Full heat comes early. When the SCRs fire at the power factor angle, the current is already a full sine wave. Firing any earlier adds nothing. On the lower chart, that is the flat part at the right. Many weld controls have a power factor setting for this reason.

Firing delay vs. conduction angle. Firing delay is how long the control waits after the voltage crosses zero. Conduction angle is how long the current flows. They move in opposite directions. Many weld current meters show the conduction angle and call it the “firing angle.” It goes up as you add heat.

Every machine is different. The power factor angle depends on the transformer, the size of the throat, and any steel inside it. So the same percent heat can give different current on different machines. Constant current controls solve this. They measure the current and adjust the firing on every weld.

Simplified model for illustration. It assumes an ideal transformer, steady line voltage, and constant weld resistance. Real machines vary. Questions? Call Spot Weld at (800) 582-5229.